dc.description.abstractThe objective of this work is to determine the effect of alkaline treatment parameters on IFSS of sugar palm fiber-polyester system. Whilst the fiber was obtained from local sources, the polyester was produced by the PT Justus Kimia Raya. The parameters being studied are alkali content of the solution (0.0, 2.5, 5.0 dan 7.5 wt%), and soaking time (0, 2, 4, da 6 jam). The experiment was carried out in two stages. First, the soaking time was kept constant at 2 hrs, and the alkali content was varied. The alkali content producing the highest IFSS was then used in the second stage where the soaking time was varied. Fiber surface morphology was determine by closely observed the SEM photo micrograph of the the samples. Specimens were treated sugar palm fibers embedded at various depths in two blocks of polyester (one at each end), then axially loaded. The IFSS was obtained from those fibers who were pulled out. Cross-sectional area of the fiber were determine by beasuring their respective SEM photo micrograpgh of the samples by means of an open source software, the imageJ. It was revealed that the highest IFSS being 5.24 MPa for large fibers, and 5.04 MPa for small fibers was obtained at 2.5 wt% alkali content and 2 hrs soaking time. At higher alkali content and longer soaking time, the IFSS was found being lower that may be caused by deteriaration of cellulose microfibril at the outer layer.en_US
dc.description.sponsorshipUMYen_US
dc.publisherUniversitas Muhammadiyah Purworejoen_US
dc.subjectalkaline treatmenten_US
dc.subjectinterfacial shear strengthen_US
dc.subjectpolyesteren_US
dc.subjectsoaking timeen_US
dc.subjectsugar palm fiberen_US
dc.titleALKALINE TREATMENT FOR INTRERFACIAL SHEAR STRENGTH (IFSS) IMPROVEMENT OF SUGAR PALM FIBER-POLYESTER SYSTEMen_US
dc.title.alternativeMENINGKATKAN KUAT GESER REKATAN ANTARMUKA (IFSS) IJUK-POLIESTER DENGAN PERLAKUAN ALKALIen_US
dc.typeArticleen_US


Files in this item

Thumbnail

This item appears in the following Collection(s)

  • CONFERENCE
    Berisi artikel ilmiah (bukan sertifikat) yang ditulis oleh dosen pada acara konferensi baik lokal, nasional maupun internasional dengan penyelenggara dari luar UMY, baik sebagai peserta Call for Paper, presenter, narasumber maupun keynote speaker.

Show simple item record