dc.descriptionThis research aims is to have a better Conductive glass for DSSC. The process of making Conductive glass by the Spray and Furnice simple method and the cost is relatively low. Conductive glass is made with glass material FTO, ZnO, AlCl3, PVA and Aquades as mixtures or solvents. After ZnO and AlCl3 are dissolved with Aquades with 5 grams of ZnO doped 0.30 grams of AlCl3 and dissolved homogeneously with 10 ml of Aquades, AZO solvent is formed, and mixed with PVA solvent with variations of 1.5 grams, 1 gram, and 0.50 gram, dissolved with10 ml of Aquades. The results this study indicate that the variation of PVA 1 gram with a resistance value of 516 Ω is the best variation compared to the variation of 1.5 grams and 0.50 grams with a resistance value of 714 Ω and 517 Ω . In the study of Transmittance and Absorption test using a UV-Vis machine variation of 1 Gram PVA has a Transmittance value 56.833% and an Absorbance of 0.265 lm.en_US
dc.description.abstractThis research aims is to have a better Conductive glass for DSSC. The process of making Conductive glass by the Spray and Furnice simple method and the cost is relatively low. Conductive glass is made with glass material FTO, ZnO, AlCl3, PVA and Aquades as mixtures or solvents. After ZnO and AlCl3 are dissolved with Aquades with 5 grams of ZnO doped 0.30 grams of AlCl3 and dissolved homogeneously with 10 ml of Aquades, AZO solvent is formed, and mixed with PVA solvent with variations of 1.5 grams, 1 gram, and 0.50 gram, dissolved with10 ml of Aquades. The results this study indicate that the variation of PVA 1 gram with a resistance value of 516 Ω is the best variation compared to the variation of 1.5 grams and 0.50 grams with a resistance value of 714 Ω and 517 Ω . In the study of Transmittance and Absorption test using a UV-Vis machine variation of 1 Gram PVA has a Transmittance value 56.833% and an Absorbance of 0.265 lm.en_US
dc.publisherPROGRAM VOKASI UNIVERSITAS MUHAMMADIYAH YOGYAKARTAen_US
dc.subjectDSSC, AZO, PVA, Transmittance, Absorbanceen_US
dc.titleFABRIKASI KACA KONDUKTIF TRANSPARAN BERBAHAN DASAR AZO SEBAGAI ELEMEN DSSCen_US
dc.typeThesis SKR FT 418en_US


Files in this item

Thumbnail
Thumbnail
Thumbnail
Thumbnail
Thumbnail
Thumbnail
Thumbnail
Thumbnail
Thumbnail
Thumbnail
Thumbnail

This item appears in the following Collection(s)

Show simple item record