dc.descriptionPROSENTASE KEKUATAN SISA BETON ADIKTIF UNTUK VARIASI SUHU 300 DERAJAT C, 900 DERAJAT C DAN LEBIH DARI 1000 DERAJAT C BERTURUT-TURUT ADALAH SEBESAR 88,89%, 65,45%, 22,51% DAN 12,00%en_US
dc.description.abstractPROSENTASE KEKUATAN SISA BETON ADIKTIF UNTUK VARIASI SUHU 300 DERAJAT C, 900 DERAJAT C DAN LEBIH DARI 1000 DERAJAT C BERTURUT-TURUT ADALAH SEBESAR 88,89%, 65,45%, 22,51% DAN 12,00%en_US
dc.language.isootheren_US
dc.publisherFT UMYen_US
dc.subjectKUAT TEKAN BETONen_US
dc.subjectBAHAN ADITIFen_US
dc.titlePERBANDINGAN KUAT TEKAN BETON PASCA BAKAR ANTARA BETON NORMAL DAN BETON DENGAN BAHAN ADITIFen_US