dc.descriptionDARI HASIL PENELITIAN KUAT TEKAN BETON YANG DIHASILKAN MENGALAMI PENURUNAN DENGAN BERTAMBAH BESARNYA NILAI FAS YANG DIGUNAKANen_US
dc.description.abstractDARI HASIL PENELITIAN KUAT TEKAN BETON YANG DIHASILKAN MENGALAMI PENURUNAN DENGAN BERTAMBAH BESARNYA NILAI FAS YANG DIGUNAKANen_US
dc.language.isootheren_US
dc.publisherFT UMYen_US
dc.subjectFASen_US
dc.subjectBETONen_US
dc.subjectAGREGATen_US
dc.titleUJI KUAT TEKAN BETON DENGAN VARIASI FAS 0,30, 0,31, 0,32, 0,33, 0,34, 0,35 UNTUK UKURAN AGREGAT KASAR MAKSIMUM 20 MM GRADASI AGREGAT HALUS DAERAH Ien_US
dc.typeThesisen_US


Files in this item

Thumbnail
Thumbnail
Thumbnail
Thumbnail
Thumbnail
Thumbnail
Thumbnail
Thumbnail
Thumbnail

This item appears in the following Collection(s)

Show simple item record