      PERBAIKAN BALOK BETON BERTULANG DENGAN METODE JACKETING DENGAN BAHAN FEROSEMEN AKIBAT BEBAN SIKLIK PADA BEBAN ULTIMIT

      Thumbnail
      View/Open
      jurnal001.pdf (390.8Kb)
      Date
      2011-11
      Author
      SOEBANDONO, BAGUS
      TRIWIYONO, ANDREAS
      MUSLIKH, MUSLIKH
      Metadata
      Show full item record
      Abstract
      A large number of buildings construction was made of reinforced concrete structure, composed of concrete and steel. The reinforced concrete structure elements could experience damage due to earthquake, from light to heavy failure, such as heavy bending-shear crack near the beam column joint. It is necessary, therefore, to repair the structure adopted good method and workability. The specimens were part of exterior beam-column joint model. Cyclic lateral load was applied to simulate earthquake load. This research used 3 specimens: US-1, the shear damage specimen as the result of first-step loaded test, then are repaired by using 1 layer rectangular galvanized welded wire mesh became R-US.1. US-2, the shear damage specimen as the result of first-step loaded test, then are repaired by using 2 layers rectangular galvanized welded wire mesh became R-US.2. UBB, the bending damage specimen as the result of the first-step loaded test, then repaired by using 2 layers rectangular galvanized welded wire mash became R-UBB. The result showed that the retrofitted on ultimate load by using jacketing ferrocement increased the ultimate strength capacity of 91,667 % (US-1 to R-US.1), 81,818% (US-2 to R.US.2) and 28,571% (UBB to R-UBB) respectively. Increasing the hysteretic energy were 215,66% (US-1 to R-US.1), 273,11% (US-2 to R.US-2) and 389,84% (UBB to R-UBB). The ductility of retrofitted specimen 6,64 (R-US.1) and 12,72 (R-US.2). The initial stiffnes of retrofitted specimen decreased 60 % (US-1 to R-US.1), 40 % (US-2 to R-US.2) and 18 % (UBB to R-UBB). Key words: shear strength, cyclic load, retrofit
      URI
      http://repository.umy.ac.id/handle/123456789/10403
      Collections
      • JURNAL

      DSpace software copyright © 2002-2015  DuraSpace
      Contact Us | Send Feedback
      Theme by 
      @mire NV
       

       

      Browse

      All of UMY RepositoryCollectionsBy Issue DateAuthorsTitlesSubjectsThis CollectionBy Issue DateAuthorsTitlesSubjects

      My Account

      Login

      DSpace software copyright © 2002-2015  DuraSpace
      Contact Us | Send Feedback
      Theme by 
      @mire NV