View Item 
      •   UMY Repository
      • 03. DISSERTATIONS AND THESIS
      • Students
      • Undergraduate Thesis
      • Faculty of Medicine and Health Science
      • Department of Dentistry
      • View Item
      •   UMY Repository
      • 03. DISSERTATIONS AND THESIS
      • Students
      • Undergraduate Thesis
      • Faculty of Medicine and Health Science
      • Department of Dentistry
      • View Item
      JavaScript is disabled for your browser. Some features of this site may not work without it.

      PERBEDAAN KEKUATAN GESER SELF ADHESIVE SEMEN DAN SEMEN IONOMER KACA TIPE 1 PADA RESTORASI VENEER INDIREK RESIN KOMPOSIT MICROHYBRID

      Thumbnail
      View/Open
      COVER (21.29Kb)
      HALAMAN JUDUL (307.6Kb)
      HALAMAN PENGESAHAN (223.6Kb)
      ABSTRACT (87.87Kb)
      BAB I (212.3Kb)
      BAB II (201.2Kb)
      BAB III (240.2Kb)
      BAB IV (153.1Kb)
      BAB V (83.15Kb)
      DAFTAR PUSTAKA (143.8Kb)
      LAMPIRAN (568.6Kb)
      NASKAH PUBLIKASI (110.0Kb)
      Date
      2016-05-19
      Author
      HERLAN, DENURA SYABINA PUTRI
      Metadata
      Show full item record
      Abstract
      Introduction: Nowadays aesthetic treatments in dentistry is growing ,so it improve the esthetics treatment to be many ways for correct dental problem. One of the most treatment in esthertic is veneer restoration for anterior teet. Veneer restorations divided into 2 type of technique are direct and indirect, for indirect veneer restorations is the technique which performed outside the mouth such as veneer from ceramic material or resin composite and indirect veneer is performed in a laboratory . Materials function for the attached a veneer with the tooth. Resin cement RelyXtm U200 is one type of resin cement as a glass ionomer cement type I which is designed for cementation material. The importance of research in order to follow the development of science in dental aesthetic treatment and needed for further research. Objective: To study there are any difference of shear bond strength between two cementation materials. Methods: This study is experimental labolatorium by using 12 sample of post- premolar tooth extraction and divided into 2 groups with data analysis used independent sample t test. Results: The different of shear strength test were show the results of the indirect veneers cemented with RelyX dhesif in average 3,57Mpa and glass ionomer cements Type 1 2.14 Mpa. Conclusion: RelyX are resistant to shear bond strength compared to glass ionomer cement type 1.
      URI
      http://repository.umy.ac.id/handle/123456789/6342
      Collections
      • Department of Dentistry

      DSpace software copyright © 2002-2015  DuraSpace
      Contact Us | Send Feedback
      Theme by 
      @mire NV
       

       

      Browse

      All of UMY RepositoryCollectionsBy Issue DateAuthorsTitlesSubjectsThis CollectionBy Issue DateAuthorsTitlesSubjects

      My Account

      Login

      DSpace software copyright © 2002-2015  DuraSpace
      Contact Us | Send Feedback
      Theme by 
      @mire NV